Objectives: To evaluate the impact of surface conditioning of titanium, zirconia thickness, and cement type on the final color of zirconia luted to the titanium. Methods: A total of 192 grade 5 titanium specimens with the final dimensions 10 mm × 10 mm × 2 mm were fabricated and subjected to four different surface conditioning including, that is, sandblasting, etching, and anodization. In addition, 192 zirconia specimens with the same dimensions as the titanium specimens but altered …